Two green petroleum cokes obtained from Pertamina UP II Dumai, Indonesia (DG32) and from Ruhr Öl Gelsenkirchen, Germany (GG64) were utilized in these studies. The predried and ground raw materials having particle diameters of mm were dried in an oven at 110 °C for 2 h prior to activation. The activation of coke samples was ...